SGS作为全球领先的第三方实验室,福建SGS检测中心为您提供专业服务。
臭氧在大气中的含量很少却是橡胶龟裂的主要因素,臭氧老化箱模拟和强化大气中的臭氧条件,研究臭氧对橡胶的作用规律,快速鉴定和评价橡胶抗臭氧老化性能与抗臭氧剂防护效能的方法,进而采取有效的防老化措施,以提高橡胶制品的使用寿命。具体条件如下:
常规条件:
"ASTM G154-12a Cycle 1
(非金属材料)"
"ASTM D4329-13 Cycle A
(塑料, 室外)"
"ASTM D4587-11 Cycle 4
(涂料)"
GB/T 14522-2008 Cycle 1
"ASTM C1442-14 Clause 7.3
(密封胶)"
"AATCC 186-2009(R2013) Option 1
(纺织品)"
"ISO 4892-3:2013 Cycle 1
(塑料, 室外)"
"ASTM D1148-13(橡胶)
Section 7.4"
"ASTM D750-12 (橡胶)
Clause 6.8"
"ASTM D925-14 (橡胶)
Method B"
GB/T 14522-2008 Cycle 2
"GB/T 16422.3-2014 Cycle 1
(塑料)"
非常规条件:
"ASTM G154-12a Cycle 2~6,8
(非金属材料)"
"ASTM D4329-13 Cycle B,C
(塑料, 室外)"
ASTM D4587-11 Cycle 1~3(涂料)
"ASTM D5208-14 Cycle A, B, C
(光降解塑料)"
"AATCC 186:2009(R2013) Option 3
(纺织品)"
"ISO 4892-3:2013 cycle 5, 6
(塑料)"
"SAE J2020-2003
(汽车外饰件)"
"EN ISO 11507:2007 Method A
(涂料)
(已作废,被EN ISO 16474-1-2013,EN ISO 16474-3-2013取代)"
"ISO 16474-3:2013 Cycle 1, 3, 4
(涂料和清漆)"
"BS 2782 Part 5:1995 Cycle A
(塑料) "
"GB/T 16422.3-2014 Cycle 5, 6
(塑料)"
"ASTM D4674-02a(2010) Method Ⅳ
(塑料, 室内)"
GB/T 14522-2008 Cycle 3~4, 7~10
"GB/T 16585-1996
(橡胶)"
"GB/T 23983-2009
(木器漆)"
"BS EN 14836:2005
(户外体育场所人造地面)"
非常规条件:
"ASTM G154-12a Cycle 7
(非金属材料)"
"ISO 4892-3:2013 cycle 2, 3, 4
(塑料, 室外) "
"EN ISO 11507:2007 Method B
(涂料)
(已作废,被EN ISO 16474-1-2013,EN ISO 16474-3-2013取代)"
"ISO 16474-3:2013 Cycle 2, 5
(涂料和清漆)"
"AATCC 186:2009(R2013) Option 2
(纺织品)"
"GB/T 16422.3-2014 Cycle 2
(塑料)"
"EN 927-6:2006
(户外木器漆)"
"EN 12224:2000
(土工织物)"
GB/T 14522-2008 Cycle 5, 6
如需了解更多信息,请联系我司。